TLDR: A voltage curve can tell you a cell is dying. It cannot tell you the separator got nicked by a foil burr on wrap forty, or that the jelly roll was squeezed harder at the core than the outer roll. For that, you open it up. Welcome to the autopsy.

We diagnose cells almost entirely from the outside. Capacity fade, resistance rise, dQ/dV, impedance: all real, all necessary, and all blind to geometry. A cycling curve is a death certificate. It tells you the cell died and roughly when. It does not tell you why. For the why, you have to look inside, and failure analysis is one of the most overlooked skills in the whole business.

Let's get into it.

This post is not a sponsored post, we are just CT software fangirls.

Reading the roll, center to outside

Cut a cylindrical cell in half, or scan it with X-ray CT, which is the version that doesn't destroy the cell, and you see the jelly roll: a tight concentric spiral of cathode, separator, anode, separator, wound around a center pin and sealed in a steel can. An 18650 carries one set of tabs; a 4680 goes tabless to pull current off the whole edge. The cross-section shows you what no curve can. How tight the wind is. Whether the core deformed. Where the tabs landed and how well they welded. Whether the layers delaminated, and whether electrolyte actually wet the whole roll or left dry patches. Center to outside is a timeline of the wind: the core saw the tightest radius and the most stress, and the outer wraps are the loose ending.

Figure 1. A real 18650 seen end-on by X-ray CT. The bright ring is the steel can, the tight spiral is the wound jelly roll (cathode, separator, anode, separator), and the dark dot in the middle is the center mandrel. Near the core you can spot the tab and a small winding wobble, the kind of thing a voltage curve will never tell you. CT scan: Glimpse, CC BY-NC-SA 4.0.

Edge shorting, where cells stab themselves

The electrode edge is the danger zone, and the classic culprit is a burr. Slitting the metal foils can leave a microscopic whisker on the edge that, given a little pressure and time, punches through the separator and shorts the cell from the inside. Two more edge sins show up constantly. Overhang misalignment: the anode is supposed to overhang the cathode, and when registration drifts, a cathode edge ends up facing bare anode, which invites lithium plating right where you least want it. And separator shrinkage at temperature, which pulls the referee off the field at exactly the wrong moment. The fixes are unglamorous and effective: clean slitting and deburring, generous anode overhang, ceramic-coated separators, and real tension control on the winder. The nasty part is that an edge short can be latent. It passes formation, ships, and fails months later. That is precisely the kind of thing a post-cycling cross-section catches and a spec sheet never will.

Figure 2. A 4680 from the side. Layers stack top to bottom, the hollow mandrel runs up the middle, and the electrode edges crowd the very top and bottom, which is exactly where edge shorts like to start. CT scan: Glimpse, CC BY-NC-SA 4.0.

Figure 3. Where cells stab themselves. A foil burr punching through the separator, an anode/cathode overhang that drifted out of registration, and a separator that shrank back at temperature. Three small edge failures, three internal shorts.

Inhomogeneous compression, the quiet killer

Stack pressure in a wound cell is not uniform. It runs highest near the core, changes with winding tension, and shifts as the electrodes breathe during cycling. That unevenness is not cosmetic. Where pressure is high, current crowds and plating starts. Where it drops, layers delaminate and gas collects. And in high-expansion chemistries like silicon, the electrolyte itself gets shoved around, leaving salt-starved zones that age faster than their neighbors. This is why pouch and prismatic cells get clamped into fixtures while a cylindrical cell relies on the can and the wind to hold itself together, and it is why degradation in a cross-section so often clusters in one region instead of spreading evenly.

The reality check

The cell was telling you it was hurt the whole time. The data showed the symptom. Only the autopsy shows the wound. If you diagnose from curves alone, you are reading the obituary and calling it a diagnosis.

Figure 4. Uh Oh. Jelly roll deformation as a cylindrical cell cycles. Source: Glimpse

Batteries don't die of old age. They die of specific, findable, preventable things: a burr, a bad wind, a pressure gradient nobody controlled. You just have to be willing to cut one open and look. Better yet, scan it first.

Some Resources We Love:

References:

  • A. Condon et al., "A dataset of over one thousand computed tomography scans of battery cells," Data in Brief (2024). DOI: 10.1016/j.dib.2024.110614

  • P. M. Attia, A. Weng, W. C. Chueh, "Limits of electrochemical data for predicting battery lifetime and failure," Joule (2026). DOI: 10.1016/j.joule.2026.102423

  • "Visualization and Detection of Internal Damage Caused by External Mechanical Loads in Cylindrical Li-Ion Batteries," Journal of The Electrochemical Society (2026). DOI: 10.1149/1945-7111/ae5b2a

  • "Electrolyte Motion Induced Salt Inhomogeneity in Si-Containing Cylindrical Cells: A Case Study," Journal of The Electrochemical Society (2026). DOI: 10.1149/1945-7111/ae4b6e

Subscribe to keep reading

This content is free, but you must be subscribed to Battery Burn Book to continue reading.

Already a subscriber?Sign in.Not now